Shake well, mix and make a Test cardboard.
1.3 mm
2 - 3 bar
2 passages = 40 μm
Number of layers
2-3 layers
Time between
coats
5 - 10 min / 20°C
Drying time
2 hours / 20°C
Mixing
10-15% Max. of Thinner
FINISH
Ready to use, after mixing Hardener and Thinner.